Sharee J. McNab, Richard J. Blaikie
Materials Research Society Symposium - Proceedings
A dielectric relaxation peak is reported in BaTiO3 and in BaTi1-xFexO3. It is nearly monodispersive, centered in the 108-Hz range, and slowest at the transition temperature Tc 413 K from the cubic to the tetragonal phase. Iron doping lowers Tc and slows down this relaxation mode. © 1989 The American Physical Society.
Sharee J. McNab, Richard J. Blaikie
Materials Research Society Symposium - Proceedings
Robert W. Keyes
Physical Review B
B.A. Hutchins, T.N. Rhodin, et al.
Surface Science
O.F. Schirmer, W. Berlinger, et al.
Solid State Communications