About cookies on this site Our websites require some cookies to function properly (required). In addition, other cookies may be used with your consent to analyze site usage, improve the user experience and for advertising. For more information, please review your options. By visiting our website, you agree to our processing of information as described in IBM’sprivacy statement. To provide a smooth navigation, your cookie preferences will be shared across the IBM web domains listed here.
Publication
ECTC 2009
Conference paper
The over-bump applied resin wafer-level underfill process: Process, material and reliability
Abstract
The over bump applied resin (OBAR) process is a waferlevelunderfill (WLUF) process in which a filled resin is applied over the bumps of a wafer and, dried. The wafer is diced into coated chips which are aligned and joined to a substrate resulting in an underfilled flip chip package. This process has been evaluated by IBM on several test vehicles in close cooperation with Henkel (formerly Abelstik) who developed a material specifically to fit this process. The critical steps to make this technology work are alignment of OBAR coated chip to a substrate, elimination of significant voids, formation of a fillet with appropriate shape and size, fluxing and solder joining. . The reliability of the material was evaluated after capping and BGA (Ball Grid Array) attach through JEDEC level 3 preconditioning followed by DTC (deep thermal cycling), T&H (temperature and humidity), and HTS (high temperature storage). While some improvements are still needed, the OBAR process has been shown to be a viable alternat ve to capillary underfill application. © 2009 IEEE.