About cookies on this site Our websites require some cookies to function properly (required). In addition, other cookies may be used with your consent to analyze site usage, improve the user experience and for advertising. For more information, please review your options. By visiting our website, you agree to our processing of information as described in IBM’sprivacy statement. To provide a smooth navigation, your cookie preferences will be shared across the IBM web domains listed here.
Publication
Thin Solid Films
Paper
The use of in situ X-ray diffraction, optical scattering and resistance analysis techniques for evaluation of copper diffusion barriers in blanket films and damascene structures
Abstract
Three in situ analysis techniques consisting of X-ray diffraction, elastic light scattering and resistance analysis have been used to investigate the failure temperatures of Cu diffusion barriers. Bilayer films consisting of 200 nm Cu on a 20-24-nm barrier (Ta, Ti7W93, Ta36Si12N52, TiN) on single and polycrystalline Si were analyzed as blanket layers and in damascene structures. The damascene structures were trenches with SiO2/Si side walls and Si(100) bottoms 0.6 μm deep, 0.23-0.62 μm in width (aspect ratios 0.97-2.6) and 5.1-80 μm in length. Barrier failure was determined by using the three techniques to monitor Cu silicide formation, which occurs at low temperatures <250°C when Cu is in direct contact with an unlimited supply of Si. The barriers were annealed at a temperature ramp rate of 3°C/s from 100 to 1000°C in N2. In the first analysis method, failure temperatures were determined by monitoring the disappearance of the Cu(111) X-ray diffraction peak and appearance of Cu silicide diffraction peaks. Simultaneously, elastic light scattering was used, where barrier failure is indicated by increases in surface roughness monitored at two different lateral length scales. Increases in sheet resistance of the blanket films on poly-Si were also monitored simultaneously using a four-point probe technique. It was determined, with the three techniques, that the order of increasing effectiveness for the barriers studied was Ta<Ti7W93<Ta36Si12 N52<TiN. It was also shown that all barriers, except TiN, show a decrease in failure temperature as trench width decreases (aspect ratio increases). © 2001 Elsevier Science B.V. All rights reserved.