About cookies on this site Our websites require some cookies to function properly (required). In addition, other cookies may be used with your consent to analyze site usage, improve the user experience and for advertising. For more information, please review your options. By visiting our website, you agree to our processing of information as described in IBM’sprivacy statement. To provide a smooth navigation, your cookie preferences will be shared across the IBM web domains listed here.
Publication
Langmuir
Paper
Influence of molecular architecture on the dewetting of thin polystyrene films
Abstract
The control of dewetting for thin polymer films is a technical challenge and of significant academic interest. We have used polystyrene nanoparticles to inhibit dewetting of high molecular weight, linear polystyrene, demonstrating that molecular architecture has a unique effect on surface properties. Neutron reflectivity measurements were used to demonstrate that the nanoparticles were uniformly distributed in the thin (ca. 40 nm) film prior to high temperature annealing, yet after annealing, they were found to separate to the solid substrate, a silanized silicon wafer. Dewetting was eliminated when the nanoparticles separated to form a monolayer or above while below this surface coverage the dewetting dynamics was severely retarded. Blending linear polystyrene of similar molecular weight to the polystyrene nanoparticle with the high molecular weight polystyrene did not eliminate dewetting. © 2005 American Chemical Society.